D3 tool steel round bar/plate

Here's what we're working on and thinking about at Vincie.web

Products | Tool Die Steels | D3 tool steel round bar/plate

D3 tool steel round bar/plate



D3 tool steel round bar plate


Delivery Date


Delivery status: Hot-Rolled 、Forged 、
Surface: Blank 、Polished 、
Standard: AISI
Shape: Round, Flat, Square, Hexagon, Plate, Sheet, Other


Specifications

Timely delivery and competitive price

strict quality control system

Annealed+Peeled

EAF Hot forged

Flexible MOQ

Product description

1.Chemical Composition(%)

steel grade

C

Si

Mn

Cr

Mo

V

Cr12

2.00-2.30

≤0.40

≤0.40

11.5-13.0

-

-

DIN 1.2080

1.90-2.20

0.10-0.40

0.15-0.45

11.0-12.0

-

-

JIS SKD1

1.80-2.40

≤0.40

≤0.60

12.0-15.0

-

≤0.30

AISI D3

2.00-2.35

0.25-0.45

0.24-0.45

11.0-13.0

0.8

0.8

2.Properties

• good wear resistance and compressive strength

• resistance to plastic deformation

• good hardenability

3. Application

Cr12 Cold Work Steel is used in high stressed cutting and punching tools for thin sheets, drawing and deep drawing tools ,stone processing tools, knives for paper and plastics, shear knives for thin sheets ,thread rolling dies.

4.Technical Route

EAF+LF+Forging+(Rolling)+Annealing Condition (optional)

5.Size available

Round bar dia     50-500mm

Flat thickness  30-300mm width100-600mm

6.Ultrasonic Test

Ultrasonic test according to SEP 1921-84 D/d

7.Delivery condition

Annealed + black/peeled/turned/grinding/polishing surface upon customers' special request

Packing & Delivery

Packaging Detail:

By bundle or upon customer's special request

Delivery Detail:

45-60 days upon quantity requirement

D3 tool steel round bar/plate Range of products
Product type Products Dimension Processes
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded

Enquiry