Grades | Tool Die Steels | D3

ASTM D3

PDF | Word | Print

D3 Application:Cold-Work Tool Steel

Chemical composition(mass fraction)(wt.%) of the D3
Elements Min.(≥) Max.(≤) Similar Remarks
C 2.00 2.35
Si 0.10 0.60
Mn 0.20 0.60
P - 0.030
S - 0.030
Cr 11.00 13.50
Mo - -
V - 1.00
W - 1.00
Ni+Cu - 0.75

Mechanical properties of grade D3

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
494 (≥) 592 (≥) 24 22 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 221

Physical properties of grade D3

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
249 (≥) 181 (≥) 44 31 13 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
614 898 738 - - -

D3 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED