| P20+Ni round bars | ||||||
| Chemical Composition(%) | ||||||
| C | Si | Mn | P | S | Cr | Mo |
| 0.28-0.40 | 0.20-0.80 | 0.60-1.00 | ≤0.030 | ≤0.030 | 1.40-2.10 | 0.30-0.50 |
| Use | ||||||
| Used for various large-sized or medium-sized precision plastic mould and low melting point alloy parts,like tim,zinc and Lead alloy casting mould. | ||||||
| Hardness | ||||||
| Hardened&Tempering,
Hardness:28-34HRC,Annealing,hardenss:HBS≤235. |
||||||
| Melting Process | ||||||
| 1. EAF: Electric Furnace+LF+VD(Optional) | ||||||
| 2. ESR: Electric Furnace+LF+VD+Eleroslag Remelted(Optional) | ||||||
| UT Class | ||||||
| According to Standard of SEP 1921/84,100% Volume, Level C/c, D/d or E/e | ||||||
| Tolerance on Quantity | ||||||
| +/-10% Per Size | ||||||
| Product type | Products | Dimension | Processes |
|---|---|---|---|
| Plates / Sheets | Plates / Sheets | 0.08-200mm(T)*W*L | Forging, hot rolling and cold rolling |
| Steel Bar | Round Bar, Flat Bar, Square Bar | Φ8-1200mm*L | Forging, hot rolling and cold rolling, Cast |
| Coil / Strip | Steel Coil /Steel Strip | 0.03-16.0x1200mm | Cold-Rolled & Hot-Rolled |
| Pipes / Tubes | Seamless Pipes/Tubes, Welded Pipes/Tubes | OD:6-219mm x WT:0.5-20.0mm | Hot extrusion, Cold Drawn, Welded |