The Stocl of the 1.2601
| Steel grade | Dimension | Shape | Unit | Quantity | Delivery state | |
|---|---|---|---|---|---|---|
| 1.2601 | 12-160(T)*310-610(W)*L | Plate or Sheet | Tons | 11.22 | Hot-Rolled+Annealed+black | |
Equivalent Grade |
||||||
| GB 2Cr12MoVNbN | DIN 1.2379 | ASTM D3 | DIN X165CrMoV12 | DIN 1.2601 | JIS SKD-11 | SS SS 2310 | GOST X12M | AFNOR X160CrMoV12 / Z160CDV12 | | ||||||
Equivalent Products |
||||||
| ASTM SKD-11 Cold working die steel | UNS D2(Cr12Mo1V1) Hot Rolled Plate | ASTM SKD11(D2, 1.2379, X153CrMo12) Cold Work Tool Steel | ASTM X165CrMoV12 Cold working die steel | | ||||||