Grades | Stainless Steels | X3CrNiMo17-13-3, 1.4436, X2CrNiMo18-14-3, 1.4435, 1.4432, X2CrNiMo17-12-3
Whole X3CrNiMo17-13-3, 1.4436, X2CrNiMo18-14-3, 1.4435, 1.4432, X2CrNiMo17-12-3 ( Austenite )
PDF | Word | Print
X3CrNiMo17-13-3, 1.4436, X2CrNiMo18-14-3, 1.4435, 1.4432, X2CrNiMo17-12-3 Application:The products in these steel grades are commonly used in the manufacture of pumps, tanks for chemicals, pipelines and installations, heat exchangers, screws, nuts, special coolers, food, chemical, textile, paper and cryogenic equipment, oil and marine indu
| Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
|---|---|---|---|---|
| C | - | 0.05 | ||
| Mn | - | 2.00 | ||
| Si | - | 1.00 | ||
| P | - | 0.045 | ||
| S | - | 0.015 | ||
| Cr | 16.50 | 18.50 | ||
| Ni | 10.50 | 13.00 | ||
| Mo | 2.50 | 3.00 | ||
| N | - | 0.10 |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | HBW |
|---|---|---|---|---|---|---|
| 681 (≥) | 591 (≥) | 41 | 21 | 41 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 243 |
| Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
|---|---|---|---|---|---|
| 693 (≥) | 958 (≥) | 32 | 13 | 43 | Solution and Aging, Annealing, Ausaging, Q+T,etc |
| Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
- | - | - |
| 696 | 647 | 518 | - | - | - |
| Product type | Products | Dimension | Processes | Deliver Status |
|---|---|---|---|---|
| Plates / Sheets | Plates / Sheets | 0.08-200mm(T)*W*L | Forging, hot rolling and cold rolling | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting |
| Steel Bar | Round Bar, Flat Bar, Square Bar | Φ8-1200mm*L | Forging, hot rolling and cold rolling, Cast | Black, Rough Turning, Shot Blasting, |
| Coil / Strip | Steel Coil /Steel Strip | 0.03-16.0x1200mm | Cold-Rolled & Hot-Rolled | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting |
| Pipes / Tubes | Seamless Pipes/Tubes, Welded Pipes/Tubes | OD:6-219mm x WT:0.5-20.0mm | Hot extrusion, Cold Drawn, Welded | Annealed, Solution and Aging, Q+T, ACID-WASHED |