Grades | Stainless Steels | 0Cr19Ni10NbN

GB 0Cr19Ni10NbN ( Austenite )

PDF | Word | Print

0Cr19Ni10NbN Application:Based on zero cr19ni9 plus N and Nb, with better than 0 cr19ni9 properties and USES

Chemical composition(mass fraction)(wt.%) of the 0Cr19Ni10NbN
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 2.00
P - 0.035
S - 0.030
Ni 7.50 10.50
Cr 18.00 20.00
Nb - 0.15
N 0.15 0.30

Mechanical properties of grade 0Cr19Ni10NbN

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
829 (≥) 436 (≥) 42 24 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 342

Physical properties of grade 0Cr19Ni10NbN

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
779 (≥) 559 (≥) 41 11 31 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
152 757 646 - - -

0Cr19Ni10NbN Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED