Grades | Stainless Steels | 22-11-2.5

GOST 22-11-2.5

PDF | Word | Print

22-11-2.5 Application:Russia TY standard grades and chemical compositions of the high temperature alloy castings

Chemical composition(mass fraction)(wt.%) of the 22-11-2.5
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.10 0.25
Cr 20.00 23.00
Al - -
Mo - -
Ti - 0.20
Co - -
W 2.40 3.00
Ni 10.50 12.50
Nb - -
Fe - -
B - -
Ce - -
V - -
Zr - -
Mn 0.60 1.20
Si 0.60 1.50
S - 0.025
P - 0.025

Mechanical properties of grade 22-11-2.5

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
946 (≥) 579 (≥) 44 22 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 133

Physical properties of grade 22-11-2.5

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
858 (≥) 887 (≥) 33 23 11 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
453 666 542 - - -

22-11-2.5 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED