Grades | Stainless Steels | X5CrNiCuNb16-4

B.S. X5CrNiCuNb16-4 ( Precipitation-Hardening )

PDF | Word | Print

X5CrNiCuNb16-4 Application:Open die steel forgings for general engineering purposes - Part 4: Stainless steels

Chemical composition(mass fraction)(wt.%) of the X5CrNiCuNb16-4
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.07
Si - 0.70
Mn - 1.50
P - 0.04
S - 0.015
Cr 15.00 17.00
Ni 3.00 5.00
Mo - 0.60
Nb+Ta 5×C 0.45
Cu 3.00 5.00

Mechanical properties of grade X5CrNiCuNb16-4

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
461 (≥) 435 (≥) 12 14 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 334

Physical properties of grade X5CrNiCuNb16-4

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
784 (≥) 198 (≥) 22 12 24 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
987 475 932 - - -

X5CrNiCuNb16-4 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED