Grades | Stainless Steels | HS 556

UNS HS 556 ( Precipitation-Hardening )

PDF | Word | Print

HS 556 Application:Alloy, Corrosion and Heat-Resistant, Sheet, Strip, and Plate 29Fe - 22Cr - 21Ni - 18.5Co - 3.2Mo - 2.8W - 0.78Ta - 0.30Al - 0.05Zr - 0.05La - 0.20N Solution Heat Treated

Chemical composition(mass fraction)(wt.%) of the HS 556
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.05 0.15
Si 0.20 0.80
Mn 0.50 2.00
Ni 19.00 22.50
Cr 21.00 23.00
Al 0.10 0.50
Cu - -
Ti - -
Fe - remaining
Mo 2.50 4.00
Co 16.00 21.00
W 2.00 3.50

Mechanical properties of grade HS 556

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
183 (≥) 317 (≥) 22 33 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 124

Physical properties of grade HS 556

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
523 (≥) 271 (≥) 33 11 11 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
794 543 366 - - -

HS 556 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED