Grades | Stainless Steels | AF 1410

ASTM AF 1410 ( Precipitation-Hardening )

PDF | Word | Print

AF 1410 Application:Steel, Bars and Forgings 2.0Cr - 10Ni - 14Co - 1.0Mo (0.15 - 0.19C) Vacuum Melted, Normalized and Overaged

Chemical composition(mass fraction)(wt.%) of the AF 1410
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.13 0.17
Si - 0.10
Mn - 0.10
P - 0.008
S - 0.005
Ni 9.50 10.50
Cr 1.80 2.20
Al - 0.015
Cu - -
Ti - 0.015
Fe - -
N - 0.0015
Mo 0.90 1.10
W - -
O - 0.0015
Co 13.50 14.50

Mechanical properties of grade AF 1410

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
641 (≥) 392 (≥) 12 32 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 132

Physical properties of grade AF 1410

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
511 (≥) 811 (≥) 44 23 12 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
812 254 459 - - -

AF 1410 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED