- GB 0Cr13A1
- GB 2Cr25N
- GB 1Cr25Ni20Si2
- GB 1Cr20Ni14Si2
- GB 2Cr20Mn9Ni2Si2N
- GB 3Cr18Mn12Si2N
- GB 0Cr15Ni25Ti2MoA1VB
- GB 1Cr16Ni35
- GB 2Cr25Ni20
- GB 2Cr23Ni13
- GB 2Cr21Ni12N
- GB 5Cr21Mn9Ni4N
- GB 4Cr14Ni14W2Mo
- GB 0Cr15Ni7Mo2Al
- GB 0Cr17Ni7Al
- GB 0Cr17Ni4Cu4Nb
- GB 3Cr16
- GB 9Cr18MoV
- GB 9Cr18Mo
- GB Y11Cr17
- GB 11Cr17
- GB 9Cr18
- GB 8Cr17
- GB 7Cr17
- GB 1Cr17Ni2
- GB 4Cr13
- GB 3Cr13Mo
- GB Y3Cr13
- GB Y3Cr13
- GB 3Cr13
- GB 2Cr13
- GB 1Cr13Mo
- GB Y1Cr13
- GB 0Cr13
- GB 1Cr13