Grades | Stainless Steels | 2Cr21Ni12N

GB 2Cr21Ni12N ( Austenite )

PDF | Word | Print

2Cr21Ni12N Application:Heat-resisting steel bars

Chemical composition(mass fraction)(wt.%) of the 2Cr21Ni12N
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.15 0.28
Si 0.75 1.25
Mn 1.00 1.60
P - 0.35
S - 0.03
Ni 10.50 12.50
Cr 20.00 22.00
N 0.15 0.30

Mechanical properties of grade 2Cr21Ni12N

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
289 (≥) 827 (≥) 41 33 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 321

Physical properties of grade 2Cr21Ni12N

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
159 (≥) 175 (≥) 33 22 34 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
817 595 298 - - -

2Cr21Ni12N Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED