SKD11(D2, 1.2379, X153CrMo12) Cold Work Tool Steel

Here's what we're working on and thinking about at Vincie.web

Products | Tool Die Steels | SKD11(D2, 1.2379, X153CrMo12) Cold Work Tool Steel

SKD11(D2, 1.2379, X153CrMo12) Cold Work Tool Steel



SKD11(D2, 1 2379, X153CrMo12) Cold Work Tool Steel is a high carbon, high chromium tool steel (12% chrome) with extremely high wear resisting properties, heat treatable to 60-62 Rc SKD11(D2, 1 2379, X153CrMo12) Cold Work Tool Steel is very wear resistant


Delivery Date


Delivery status: Forged 、Q+T 、
Surface: Milling 、
Standard: JIS
Shape: Round, Flat, Square, Hexagon, Plate, Sheet, Other


SKD11(D2, 1.2379, X153CrMo12) Cold Work Tool Steel is a high carbon, high chromium tool steel (12% chrome) with extremely high wear resisting properties, heat treatable to 60-62 Rc. SKD11(D2, 1.2379, X153CrMo12) Cold Work Tool Steel is very wear resistant but not as tough as lower alloyed steels. SKD11(D2, 1.2379, X153CrMo12) Cold Work Tool Steel hardens in air with a low order of movement and offers a measure of corrosion resistance when polished. The high percentage of chromium gives it mild corrosion-resisting properties in the hardened condition. The mechanical properties of SKD11(D2, 1.2379, X153CrMo12) Cold Work Tool Steel are very sensitive to heat treatment. SKD11(D2, 1.2379, X153CrMo12) Cold Work Tool Steel is available in de-carb free rounds, flats, and squares, as well as ground flat stock and drill rod.

USA German Japan
ASTM A681 DIN EN ISO 4957 JIS G4404
D2 1.2379/X153CrMo12 SKD11

SKD11(D2, 1.2379, X153CrMo12) Cold Work Tool Steel Mechanical Properties
Mechanical Properties Metric Imperial
Hardness, Knoop (converted from Rockwell C hardness) 769 769
Hardness, Rockwell C 62 62
Hardness, Vickers 748 748
Izod impact unnotched 77.0 J 56.8 ft-lb
Poisson’s ratio 0.27-0.30 0.27-0.30
Elastic modulus 190-210 GPa 27557-30457 ksi


SKD11(D2, 1.2379, X153CrMo12) Cold Work Tool Steel Range of products
Product type Products Dimension Processes
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded