1 2581(H21, X30WCrV93, SKD5) Hot-Work Mould Steel properties:Tungsten-chrome-vanadium steel for hardening in oil and possibly in air with very good hardenability, very high firmness during the heat and resistance to the tempering, high resistance to the


Delivery Date


Delivery status: Forged 、Q+T 、
Surface: Milling 、
Standard: DIN
Shape: Round, Flat, Square, Hexagon, Plate, Sheet, Other


Standards DIN AISI JIS ГОСТ
X30WCrV93 1.2581 H21 SKD5 3X2B8Φ

1.2581(H21, X30WCrV93, SKD5) Hot-Work Mould Steel properties:
Tungsten-chrome-vanadium steel for hardening in oil and possibly in air with very good hardenability, very high firmness during the heat and resistance to the tempering, high resistance to the hot tempering and good toughness. Further the steel has a lower resistance to tearing of thermal fatigue and higher sensitivity to quick changes of temperature. The steel is not appropriate for tools cooled by water. It is well-workable during the heat and well-workable in the soft-annealed state.

1.2581(H21, X30WCrV93, SKD5) Hot-Work Mould Steel Applications
Tools for hot mechanical working such as highly stressed small pressing dies and die inserts especially for die forging of accurate products from the difficult-workable steels and copper alloys, thorns and jaws for forging presses, forgings for swaging, tools for production of rivets, nuts and screws, small extrusion dies (matrices), thorns, pressing discs for extrusion of alloys of non-ferrous metals.

1.2581(H21, X30WCrV93, SKD5) Hot-Work Mould Steel Heat Treatment:

Soft annealing

Temperature(°C)

Cooling

Hardness

740 - 780

furnace

max. 241 HB

 

Forging

Temperature(°C)

Cooling

 

 

850 - 1100

furnace

 

 

Hardening

Temperature(°C)

Cooling

Tempering

 

1140 - 1160

oil or air

see tempering diagram


1.2581(H21, X30WCrV93, SKD5) Hot-Work Mould Steel Range of products
Product type Products Dimension Processes
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded