Grades | Superalloys | Nickel 200
ASTM Nickel 200
PDF | Word | Print
Nickel 200 Application:Acid or alkaline food production (fruit juices, ice-creams), cristallization and concentration of mineral salts. Concentration of caustic salts. Machineries in which hydrocarbons are in reaction with fluorides. Storing and carriage of phenol. Production o
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.15 | ||
Si | - | 0.35 | ||
Mn | - | 0.35 | ||
S | - | 0.01 | ||
Ni | 99 | - | ||
Cu | - | 0.25 | ||
Fe | - | 0.40 | ||
Mg | - | 0.20 | ||
Ti | - | 0.10 | ||
Co | - | 2.00 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | HBW |
---|---|---|---|---|---|---|
598 (≥) | 597 (≥) | 23 | 13 | 41 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 241 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
---|---|---|---|---|---|
551 (≥) | 224 (≥) | 32 | 12 | 34 | Solution and Aging, Annealing, Ausaging, Q+T,etc |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
- | - | - |
844 | 151 | 753 | - | - | - |
Product type | Products | Dimension | Processes | Deliver Status |
---|---|---|---|---|
Plates / Sheets | Plates / Sheets | 0.08-200mm(T)*W*L | Forging, hot rolling and cold rolling | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting |
Steel Bar | Round Bar, Flat Bar, Square Bar | Φ8-1200mm*L | Forging, hot rolling and cold rolling, Cast | Black, Rough Turning, Shot Blasting, |
Coil / Strip | Steel Coil /Steel Strip | 0.03-16.0x1200mm | Cold-Rolled & Hot-Rolled | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting |
Pipes / Tubes | Seamless Pipes/Tubes, Welded Pipes/Tubes | OD:6-219mm x WT:0.5-20.0mm | Hot extrusion, Cold Drawn, Welded | Annealed, Solution and Aging, Q+T, ACID-WASHED |