SKD-11 Cold working die steel



SKD11 high wear-resisting ductile general cold work die steel, high carbon high chromium alloy tool steel and vacuum degassing refined steel


Delivery Date


Delivery status: Hot-Rolled 、Forged 、Hot-Rolled 、 、
Surface: Blank 、Peeled 、Milling 、
Standard: JIS
Shape: Round, Flat, Square, Hexagon, Plate, Sheet, Other


SKD11 high wear-resisting ductile general cold work die steel, high carbon high chromium alloy tool steel and vacuum degassing refined steel, steel purity, has good hardenability, quenching deformation small good hardenability.The steel after spheroidizing annealing softening, machinability is good, the carbide particles small even, do not need to worry about the quenching crack strengthening elements molybdenum and vanadium are joined.
High hardness, high wear resistant uniform eutectic carbides, good toughness, not easy craze, > 62 HRC hardness after quenching.At 525 ℃ nitriding processing time for 20 h/h/h, 60 ammoniation layer depth of 0.25 mm / 0. 30 mm / 0. 35 mm, the surface hardness is 1250 hv,At 570 ℃ nitriding processing time is 2 h, nitriding depth 10 ~ 20 microns, the surface hardness is 950 hv.

Si ≤0.40

Mn  ≤0.60

P ≤0.030

S ≤0.030

Cr  11.0-13.0

Mo 0.80-1.20

Ni ≤0.50

V  0.20-0.50

Cu ≤0.25

SKD-11 Cold working die steel Range of products
Product type Products Dimension Processes
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded