Grades | Superalloys | 1.6359
DIN 1.6359 ( Martensite )
PDF | Word | Print
1.6359 Application:Structural and constructional steels
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.03 | ||
Ni | 17.00 | 19.00 | ||
Co | 7.00 | 8.50 | ||
Mn | - | 0.10 | ||
Si | - | 0.10 | ||
Al | 0.05 | 0.15 | ||
Mo | 4.60 | 5.20 | ||
S | - | 0.010 | ||
P | - | 0.010 | ||
Ti | 0.30 | 0.50 | ||
Fe | - | Bal | ||
Cr | - | 0.50 | ||
Cu | - | 0.50 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | HBW |
---|---|---|---|---|---|---|
424 (≥) | 217 (≥) | 33 | 44 | 23 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 442 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
---|---|---|---|---|---|
139 (≥) | 924 (≥) | 12 | 12 | 24 | Solution and Aging, Annealing, Ausaging, Q+T,etc |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
- | - | - |
439 | 396 | 691 | - | - | - |
Product type | Products | Dimension | Processes | Deliver Status |
---|---|---|---|---|
Plates / Sheets | Plates / Sheets | 0.08-200mm(T)*W*L | Forging, hot rolling and cold rolling | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting |
Steel Bar | Round Bar, Flat Bar, Square Bar | Φ8-1200mm*L | Forging, hot rolling and cold rolling, Cast | Black, Rough Turning, Shot Blasting, |
Coil / Strip | Steel Coil /Steel Strip | 0.03-16.0x1200mm | Cold-Rolled & Hot-Rolled | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting |
Pipes / Tubes | Seamless Pipes/Tubes, Welded Pipes/Tubes | OD:6-219mm x WT:0.5-20.0mm | Hot extrusion, Cold Drawn, Welded | Annealed, Solution and Aging, Q+T, ACID-WASHED |