Grades | Stainless Steels | S30803

AISI S30803 ( Austenite )

PDF | Word | Print

S30803 Application:Austenitic wire for metal inert gas welding. It is suitable for welding corrosion resistant 18/8 CrNi steels for devices, vessels and parts in chemical, pharmacy and cellulose industry for temperature up to 350°C. Welded material has oxidation resistance

Chemical composition(mass fraction)(wt.%) of the S30803
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.025
Si - 0.40
Mn - 1.75
P - 0.045
S - 0.03
Cr 19.0 21.0
Ni 10.00 12.0

Mechanical properties of grade S30803

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
139 (≥) 554 (≥) 34 13 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 212

Physical properties of grade S30803

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
681 (≥) 687 (≥) 12 24 23 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
465 923 574 - - -

S30803 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED