Grades | Stainless Steels | S42800

UNS S42800

PDF | Word | Print

S42800 Application:S42800

Chemical composition(mass fraction)(wt.%) of the S42800
Elements Min.(≥) Max.(≤) Similar Remarks
c 1.05 1.15
Si 0.20 0.40
Mn 0.25 0.50
P - 0.015
S - 0.01
Cr 13.7 14.8
Ni - 0.35
Mo 1.90 2.25
V 0.90 1.15
Nb 0.25 0.35
Cu - 0.35

Mechanical properties of grade S42800

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
429 (≥) 749 (≥) 34 43 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 424

Physical properties of grade S42800

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
191 (≥) 952 (≥) 14 22 32 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
339 953 756 - - -

S42800 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED