BЖЛ18-BИ Application:Russia GOCT Standard vacuum smelting casting high temperature alloy bar

Chemical composition(mass fraction)(wt.%) of the BЖЛ18-BИ
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.10 0.15
Cr 17.00 18.00
Ni - remaining
Co 4.00 6.00
Mo 4.50 6.00
W 2.50 4.00
Al 3.40 4.00
Ti 2.20 3.00
Nb 1.20 1.80
Fe - 1.00

Mechanical properties of grade BЖЛ18-BИ

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
126 (≥) 851 (≥) 23 32 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 143

Physical properties of grade BЖЛ18-BИ

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
822 (≥) 324 (≥) 22 12 22 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
115 148 666 - - -

BЖЛ18-BИ Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED