Grades | Stainless Steels | ЖC6y-BИ

GOST ЖC6y-BИ

PDF | Word | Print

ЖC6y-BИ Application:Russia GOCT Standard vacuum smelting casting high temperature alloy bar

Chemical composition(mass fraction)(wt.%) of the ЖC6y-BИ
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.13 0.20
Cr 8.00 9.50
Ni - remaining
Co 9.00 10.50
Mo 1.20 2.40
W 9.50 11.00
Al 5.10 6.00
Ti 2.00 2.90
Nb 0.80 1.20
Fe - 1.00

Mechanical properties of grade ЖC6y-BИ

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
761 (≥) 815 (≥) 31 21 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 234

Physical properties of grade ЖC6y-BИ

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
317 (≥) 811 (≥) 33 31 44 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
232 393 195 - - -

ЖC6y-BИ Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED