Grades | Stainless Steels | XH77TЮPy

GOST XH77TЮPy

PDF | Word | Print

XH77TЮPy Application:Russia GOCT standard deformation of high temperature alloy grades and chemical composition

Chemical composition(mass fraction)(wt.%) of the XH77TЮPy
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04 0.08
Si - 0.60
Mn - 0.40
P - -
S - -
Cr 19.00 22.00
Ni - remaining
Mo - -
Al 0.70 1.00
Ti 2.60 2.90
Fe - 1.00
B - 0.010
Ce - 0.02
Pb - 0.001

Mechanical properties of grade XH77TЮPy

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
788 (≥) 224 (≥) 13 32 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 212

Physical properties of grade XH77TЮPy

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
578 (≥) 647 (≥) 33 34 13 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
279 658 919 - - -

XH77TЮPy Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED