Grades | Stainless Steels | XH38BT

GOST XH38BT

PDF | Word | Print

XH38BT Application:Russia GOCT standard deformation of high temperature alloy grades and chemical composition

Chemical composition(mass fraction)(wt.%) of the XH38BT
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.06 0.12
Si - 0.80
Mn - 0.70
P - 0.030
S - 0.020
Cr 20.00 23.00
Ni 35.00 39.00
Mo - -
Al - 0.50
Ti 0.70 1.20
Fe - -
W 2.80 3.50
Ce - 0.05

Mechanical properties of grade XH38BT

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
358 (≥) 833 (≥) 32 31 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 434

Physical properties of grade XH38BT

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
775 (≥) 439 (≥) 14 13 13 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
664 972 346 - - -

XH38BT Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED