Grades | Stainless Steels | 25X18H10B2

GOST 25X18H10B2

PDF | Word | Print

25X18H10B2 Application:Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(mass fraction)(wt.%) of the 25X18H10B2
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.21 0.28
Si 0.30 0.80
Mn - 0.70
P - 0.030
S - 0.030
Cr 17.00 19.00
Ni 9.00 11.00
Mo - 0.30
W 2.00 2.50

Mechanical properties of grade 25X18H10B2

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
377 (≥) 812 (≥) 42 32 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 344

Physical properties of grade 25X18H10B2

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
725 (≥) 984 (≥) 21 21 14 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
899 368 425 - - -

25X18H10B2 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED