Grades | Stainless Steels | 10X15H9C3Б1

GOST 10X15H9C3Б1 ( Austenite )

PDF | Word | Print

10X15H9C3Б1 Application:Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(mass fraction)(wt.%) of the 10X15H9C3Б1
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.08 0.12
Si 2.20 3.00
Mn 0.40 0.80
P - 0.035
S - 0.025
Cr 14.00 16.00
Ni 8.00 10.00
Mo 3.00 4.00
W 2.00 2.75
Nb 0.90 1.30
Cu - 0.20
Zr - 0.10

Mechanical properties of grade 10X15H9C3Б1

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
395 (≥) 235 (≥) 34 21 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 142

Physical properties of grade 10X15H9C3Б1

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
769 (≥) 169 (≥) 34 42 41 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
415 573 167 - - -

10X15H9C3Б1 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED