Grades | Stainless Steels | 10X13Γ18Д

GOST 10X13Γ18Д ( Austenite )

PDF | Word | Print

10X13Γ18Д Application:Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(mass fraction)(wt.%) of the 10X13Γ18Д
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.08 0.12
Si - 0.70
Mn 17.00 18.50
P - 0.035
S - 0.030
Cr 12.50 14.00
Ni - 0.90
Mo - 0.30

Mechanical properties of grade 10X13Γ18Д

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
639 (≥) 844 (≥) 21 41 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 433

Physical properties of grade 10X13Γ18Д

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
641 (≥) 157 (≥) 24 44 34 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
511 125 768 - - -

10X13Γ18Д Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED