Grades | Stainless Steels | 04X12H2M

GOST 04X12H2M ( Austenite )

PDF | Word | Print

04X12H2M Application:Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(mass fraction)(wt.%) of the 04X12H2M
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.04
Si - 0.40
Mn 1.00 2.00
P - 0.035
S - 0.025
Cr 24.50 26.50
Ni 5.00 6.00
Mo 1.70 2.50
Ti 2.30 3.50
B 1.30 1.80
Nb - 0.20

Mechanical properties of grade 04X12H2M

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
448 (≥) 464 (≥) 43 24 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 422

Physical properties of grade 04X12H2M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
454 (≥) 982 (≥) 34 22 32 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
668 694 344 - - -

04X12H2M Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED