Grades | Stainless Steels | 45X14H1482M

GOST 45X14H1482M ( Austenite )

PDF | Word | Print

45X14H1482M Application:Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(mass fraction)(wt.%) of the 45X14H1482M
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.40 0.50
Si - 0.80
Mn - 0.70
P - 0.035
S - 0.020
Cr 13.00 15.00
Ni 13.00 15.00
Mo 0.25 0.40
W 2.00 2.80
Ti - 0.20

Mechanical properties of grade 45X14H1482M

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
231 (≥) 916 (≥) 24 24 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 213

Physical properties of grade 45X14H1482M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
582 (≥) 156 (≥) 41 32 43 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
267 398 971 - - -

45X14H1482M Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED