Grades | Stainless Steels | Z9CNA17-07

AFNOR Z9CNA17-07

PDF | Word | Print

Z9CNA17-07 Application:Iron and steel. Stainless steel for general purposes. Semi- finished products, bars and wire rod

Chemical composition(mass fraction)(wt.%) of the Z9CNA17-07
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.090
Si - 0.75
Mn - 1.00
P - 0.040
S - 0.015
Cr 16.00 17.00
Mo - -
Ni 6.50 7.75
Al 0.75 1.50

Mechanical properties of grade Z9CNA17-07

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
129 (≥) 286 (≥) 31 44 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 321

Physical properties of grade Z9CNA17-07

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
182 (≥) 144 (≥) 42 14 33 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
958 453 677 - - -

Z9CNA17-07 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED