Grades | Stainless Steels | Z6CNDNb18-12M

AFNOR Z6CNDNb18-12M

PDF | Word | Print

Z6CNDNb18-12M Application:Foundry products - Cast steel and nickel alloy castings for pumps, valves and fittings (enclosures and internal components)

Chemical composition(mass fraction)(wt.%) of the Z6CNDNb18-12M
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.060
Si - 0.75
Mn - 2.00
P - 0.040
S - 0.015
Cr 16.50 18.50
Mo 2.50 3.00
Ni 11.00 13.00
Nb+Ta 10×C 0.70

Mechanical properties of grade Z6CNDNb18-12M

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
346 (≥) 311 (≥) 23 44 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 224

Physical properties of grade Z6CNDNb18-12M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
412 (≥) 697 (≥) 23 14 24 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
384 267 148 - - -

Z6CNDNb18-12M Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED