Grades | Stainless Steels | Z3CTNb18

AFNOR Z3CTNb18

PDF | Word | Print

Z3CTNb18 Application:Iron and steel. Stainless steel for high temperature application

Chemical composition(mass fraction)(wt.%) of the Z3CTNb18
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.030
Si - 0.75
Mn - 0.08
P - 0.030
S - 0.015
Cr 17.50 18.50
Mo - -
Ni - -
N - 0.025
Ti 0.10 0.50
Nb 9×C 0.30

Mechanical properties of grade Z3CTNb18

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
358 (≥) 399 (≥) 12 13 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 244

Physical properties of grade Z3CTNb18

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
935 (≥) 224 (≥) 13 44 41 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
721 188 512 - - -

Z3CTNb18 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED