S.524 Application:Specification for cold-rolled 18/10 chromium-nickel corrosion-resisting steel sheet and strip (titanium stabilized: 800 MPa)

Chemical composition(mass fraction)(wt.%) of the S.524
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si 0.20 1.00
Mn 0.50 2.00
P - 0.035
S - 0.025
Cr 17.00 19.00
Ni 9.00 11.00
Mo - -
Ti 5×C 0.70

Mechanical properties of grade S.524

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
736 (≥) 655 (≥) 41 34 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 213

Physical properties of grade S.524

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
589 (≥) 461 (≥) 23 22 24 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
248 541 696 - - -

S.524 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED