Grades | Stainless Steels | 2S.143

B.S. 2S.143

PDF | Word | Print

2S.143 Application:Specification for high chromium-nickel corrosion-resisting steel bright bars (free machining) (880-1080 MPa: limiting ruling section 70 mm)

Chemical composition(mass fraction)(wt.%) of the 2S.143
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.07
Si - 0.60
Mn - 1.00
P - 0.035
S - 0.025
Cr 13.20 14.70
Ni 5.00 5.80
Mo 1.20 2.00
Nb 0.10 0.40
Cu 1.20 2.00

Mechanical properties of grade 2S.143

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
282 (≥) 473 (≥) 34 31 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 212

Physical properties of grade 2S.143

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
514 (≥) 284 (≥) 32 34 41 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
347 492 818 - - -

2S.143 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED