Grades | Stainless Steels | 2.4889

B.S. 2.4889

PDF | Word | Print

2.4889 Application:Heat resisting steels and nickel alloys

Chemical composition(mass fraction)(wt.%) of the 2.4889
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.05 0.12
Si 2.50 3.00
Mn - 1.00
P - 0.020
S - 0.015
Cr 26.00 29.00
Ni 45.00 -
Al - -
Fe 21.00 25.00
Cu - 0.30
Ce 0.03 0.09

Mechanical properties of grade 2.4889

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
648 (≥) 787 (≥) 14 14 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 442

Physical properties of grade 2.4889

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
523 (≥) 134 (≥) 23 31 33 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
483 845 555 - - -

2.4889 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED