1.4877 Application:Heat resisting steels and nickel alloys

Chemical composition(mass fraction)(wt.%) of the 1.4877
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04 0.08
Si - 3.00
Mn - 1.00
P - 0.020
S - 0.010
Cr 26.00 28.00
Ni 31.00 33.00
Al - 0.025
Nb+Ta 0.60 1.00
Ce 0.05 0.10
N - 0.11

Mechanical properties of grade 1.4877

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
912 (≥) 196 (≥) 23 13 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 413

Physical properties of grade 1.4877

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
255 (≥) 973 (≥) 13 23 23 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
445 195 919 - - -

1.4877 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED