Grades | Stainless Steels | 1.4335

DIN 1.4335

PDF | Word | Print

1.4335 Application:Flat products made of steels for pressure purposes - Part 7: Stainless steels

Chemical composition(mass fraction)(wt.%) of the 1.4335
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.05
Si - 0.70
Mn - 1.50
P - 0.040
S - 0.015
Cr 12.0 14.0
Mo 0.30 0.70
Ni 3.50 4.50
N - 0.020

Mechanical properties of grade 1.4335

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
557 (≥) 378 (≥) 13 13 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 211

Physical properties of grade 1.4335

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
545 (≥) 139 (≥) 31 34 24 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
928 997 274 - - -

1.4335 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED