JIS SUH 37 ( Austenite )

PDF | Word | Print

SUH 37 Application:Heat-resisting steel bars and wire rods

Chemical composition(mass fraction)(wt.%) of the SUH 37
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.15 0.25
Si - 1.00
Mn 1.00 1.60
P - 0.04
S - 0.03
Cr 20.50 22.50
Ni 10.00 12.00
Mo - -
N 0.15 0.30

Mechanical properties of grade SUH 37

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
944 (≥) 392 (≥) 42 33 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 321

Physical properties of grade SUH 37

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
351 (≥) 521 (≥) 32 11 44 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
186 211 473 - - -

SUH 37 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED