Grades | Stainless Steels | Rene 41

SAE Rene 41 ( Precipitation-Hardening )

PDF | Word | Print

Rene 41 Application:Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 53Ni - 19Cr - 11Co - 9.8Mo - 3.2Ti - 1.6Al - 0.006B Vacuum Melted, Solution Heat Treated Precipitation Hardenable

Chemical composition(mass fraction)(wt.%) of the Rene 41
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.09
Si - 0.25
Mn - 0.25
Cr - 19.00
Ni - remaining
Mo - 10.00
Co - 11.00
W - -
Al - 1.50
Cu - -
Ti - 3.10
Fe - 1.80
B - 0.005

Mechanical properties of grade Rene 41

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
211 (≥) 935 (≥) 33 14 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 224

Physical properties of grade Rene 41

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
747 (≥) 536 (≥) 22 22 43 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
129 697 739 - - -

Rene 41 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED