AMS RA 333 ( Precipitation-Hardening )

PDF | Word | Print

RA 333 Application:Nickel Alloy, Corrosion and Heat Resistant, Sheet, Strip, and Plate 45.5Ni - 25.5Cr - 3.2Co - 3.2Mo - 3.2W - 18.5Fe Solution Heat Treated

Chemical composition(mass fraction)(wt.%) of the RA 333
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.04
Si - 1.15
Mn - 1.00
Cr - 25.50
Ni - remaining
Mo - 3.25
Co - 3.00
W - 3.25
Al - -
Cu - 0.10
Ti - -
Fe - 17.00

Mechanical properties of grade RA 333

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
159 (≥) 683 (≥) 31 43 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 413

Physical properties of grade RA 333

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
227 (≥) 771 (≥) 24 24 11 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
542 859 612 - - -

RA 333 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED