Grades | Stainless Steels | UNISPAN LR 35

SAE UNISPAN LR 35 ( Precipitation-Hardening )

PDF | Word | Print

UNISPAN LR 35 Application:Wrought Nickel and Nickel-Related Alloys

Chemical composition(mass fraction)(wt.%) of the UNISPAN LR 35
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.05
Si - 0.60
Mn - 0.80
Cr - 20.00
Ni - 25.00
Mo - -
Co - -
W - -
Al - -
Cu - -
Ti - -
Fe - -
Nb - 0.60

Mechanical properties of grade UNISPAN LR 35

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
841 (≥) 461 (≥) 14 23 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 441

Physical properties of grade UNISPAN LR 35

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
642 (≥) 654 (≥) 34 33 31 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
157 584 917 - - -

UNISPAN LR 35 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED