UNS GMR-235 ( Precipitation-Hardening )

PDF | Word | Print

GMR-235 Application:Special Purpose Alloys ("Superalloys")

Chemical composition(mass fraction)(wt.%) of the GMR-235
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si - 0.30
Mn - 0.13
P - -
S - -
Ni - remaining
Cr - 15.50
Al - 3.00
Cu - -
Ti - 2.00
Fe - 10.00
Mo - 5.25
Co - -
B - 0.06

Mechanical properties of grade GMR-235

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
972 (≥) 732 (≥) 44 44 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 123

Physical properties of grade GMR-235

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
735 (≥) 178 (≥) 43 21 32 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
473 617 995 - - -

GMR-235 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED