Grades | Stainless Steels | SB-446 N06650

AMS SB-446 N06650 ( Precipitation-Hardening )

PDF | Word | Print

SB-446 N06650 Application:Nickel-Chromium-Molybdenum-Columbium Alloy (UNS N06625), Nickel-Chromium-Molybdenum-Silicon Alloy (UNS N06219), and Nickel-Chromium-Molybdenum-Tungsten Alloy (UNS N06650) Rod and Bar

Chemical composition(mass fraction)(wt.%) of the SB-446 N06650
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.01
Si - 0.05
Mn - 1.50
P - 0.04
S - 0.01
Ni - remaining
Cr 0.50 1.50
Al 0.10 0.50
Cu - 0.50
Ti - -
Fe 1.00 6.00
Mo 26.00 30.00
Co - 2.50

Mechanical properties of grade SB-446 N06650

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
292 (≥) 457 (≥) 41 31 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 324

Physical properties of grade SB-446 N06650

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
844 (≥) 634 (≥) 44 43 43 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
793 237 414 - - -

SB-446 N06650 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED