SAE B 438 CT-1000-K19 ( Precipitation-Hardening )

PDF | Word | Print

B 438 CT-1000-K19 Application:Specification for Bronze Powder Metallurgy (P/M) Bearing (Oil-Impregnated)

Chemical composition(mass fraction)(wt.%) of the B 438 CT-1000-K19
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.01
Si - 0.05
Mn - 1.50
P - 0.04
S - 0.01
Ni - remaining
Cr 0.50 1.50
Al 0.10 0.50
Cu - 0.50
Ti - -
Fe 1.00 6.00
Mo 26.00 30.00
Co - 2.50

Mechanical properties of grade B 438 CT-1000-K19

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
954 (≥) 417 (≥) 43 41 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 122

Physical properties of grade B 438 CT-1000-K19

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
686 (≥) 535 (≥) 32 23 44 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
896 918 183 - - -

B 438 CT-1000-K19 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED