AMS SA-213 TP347LN ( Precipitation-Hardening )

PDF | Word | Print

SA-213 TP347LN Application:Specification for Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes

Chemical composition(mass fraction)(wt.%) of the SA-213 TP347LN
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.005 0.02
Si - 0.75
Mn - 2.00
P - 0.04
S - 0.03
Ni 9.00 13.00
Cr 17.00 20.00
Al - -
Cu - -
Ti - -
Fe - -
N 0.06 0.10
Mo - -
V - -

Mechanical properties of grade SA-213 TP347LN

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
555 (≥) 485 (≥) 31 14 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 223

Physical properties of grade SA-213 TP347LN

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
883 (≥) 789 (≥) 12 43 33 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
594 171 978 - - -

SA-213 TP347LN Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED