Grades | Stainless Steels | A 213 TP317LMN

SAE A 213 TP317LMN ( Precipitation-Hardening )

PDF | Word | Print

A 213 TP317LMN Application:Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes

Chemical composition(mass fraction)(wt.%) of the A 213 TP317LMN
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.30
Si - 0.70
Mn - 2.00
P - 0.045
S - 0.03
Ni 13.00 27.00
Cr 18.00 20.00
Al - -
Cu - 0.75
Ti - -
Fe - -
N - 0.10
Mo 4.00 5.00
V - 0.08

Mechanical properties of grade A 213 TP317LMN

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
794 (≥) 973 (≥) 31 13 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 433

Physical properties of grade A 213 TP317LMN

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
671 (≥) 711 (≥) 44 44 22 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
846 486 261 - - -

A 213 TP317LMN Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED