Grades | Stainless Steels | A 314 XM-28

SAE A 314 XM-28 ( Austenite )

PDF | Word | Print

A 314 XM-28 Application:Stainless Steel Bars and Shapes

Chemical composition(mass fraction)(wt.%) of the A 314 XM-28
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Mn 11.0 14.0
P - 0.045
S - 0.030
Si - 1.00
Ni 0.5 2.5
Cr 16.5 19.00
N 0.20 0.45

Mechanical properties of grade A 314 XM-28

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
214 (≥) 694 (≥) 14 44 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 122

Physical properties of grade A 314 XM-28

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
826 (≥) 949 (≥) 43 43 34 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
435 943 115 - - -

A 314 XM-28 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED