Grades | Stainless Steels | HNV3

UNS HNV3

PDF | Word | Print

HNV3 Application:Steel for intake valves

Chemical composition(mass fraction)(wt.%) of the HNV3
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.40 0.50
Si 2.75 3.75
Mn - 0.80
P 0.040
S 0.03
Cr 7.50 9.50
Ni - 0.50

Mechanical properties of grade HNV3

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
185 (≥) 967 (≥) 34 14 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 121

Physical properties of grade HNV3

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
569 (≥) 695 (≥) 31 13 43 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
186 426 884 - - -

HNV3 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED