Grades | Stainless Steels | A 955 XM-29 Grade 280

SAE A 955 XM-29 Grade 280 ( Austenite )

PDF | Word | Print

A 955 XM-29 Grade 280 Application:Deformed and Plain Stainless-Steel Bars for Concrete Reinforcement

Chemical composition(mass fraction)(wt.%) of the A 955 XM-29 Grade 280
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn 11.5 14.5
P - 0.06
S - 0.03
Cr 17.0 19.0
Ni 2.25 3.75
N 0.20 0.40

Mechanical properties of grade A 955 XM-29 Grade 280

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
265 (≥) 731 (≥) 42 14 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 441

Physical properties of grade A 955 XM-29 Grade 280

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
327 (≥) 966 (≥) 43 32 32 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
189 726 735 - - -

A 955 XM-29 Grade 280 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED