Grades | Stainless Steels | A 276 S44627

SAE A 276 S44627 ( Ferrite )

PDF | Word | Print

A 276 S44627 Application:Stainless Steel Bars and Shapes

Chemical composition(mass fraction)(wt.%) of the A 276 S44627
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.01
Mn - 0.40
Si - 0.40
P - 0.02
S - 0.02
Cr 25.00 27.00
Ni - 0.50
Mo 0.75 1.50
N - 0.015
Nb 0.05 0.20
Cu - 0.20

Mechanical properties of grade A 276 S44627

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
719 (≥) 995 (≥) 24 34 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 443

Physical properties of grade A 276 S44627

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
881 (≥) 174 (≥) 44 34 13 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
759 615 324 - - -

A 276 S44627 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED