Grades | Stainless Steels | N08024

AISI N08024 ( Austenite )

PDF | Word | Print

N08024 Application:Cr-Ni-Fe-Mo-Cu Alloy Columbium Stabilized

Chemical composition(mass fraction)(wt.%) of the N08024
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Mn - 1.00
Si - 0.50
P - 0.035
S - 0.035
Cr 22.50 25.00
Ni 35.00 40.00
Mo 3.50 5.00
Cu 0.50 1.50
Nb 0.15 0.35

Mechanical properties of grade N08024

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
723 (≥) 364 (≥) 14 42 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 231

Physical properties of grade N08024

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
149 (≥) 367 (≥) 11 44 24 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
778 595 753 - - -

N08024 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED